Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 4.90 MPa | 711 psi | ISO 37 |
Multibase TPSiV® 4000-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Tensile Strength, Ultimate | >= 4.90 MPa | >= 711 psi | 80°C, 48 HS; TL VW 676 PARTE 3.4.2 |
Karina 601-48/1-BY-IS-BZ Black PVC Compound Heavy metal free, weather resistant PVC compound recommended for injection and extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength, Ultimate | 4.90 MPa | 711 psi | |
Valley Adhesives EM-800 High Temperature Application Glue Stick Valley Adhesives EM-800 High Temperature Application Glue StickGood hot tack for packaging. |
|||
Tensile Strength, Ultimate | 4.90 MPa | 711 psi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 155 FT EB Thermoplastic Vulcanizate Neoplast 155 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, .. |
|||
Tensile Strength, Ultimate | 4.90 MPa | 711 psi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 155 FT SWB Thermoplastic Vulcanizate Neoplast 155 FT SWB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant,.. |