Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 455 MPa | 66000 psi | |
PSM Industries PolyAlloys MIM-Fe-50%Ni Grade 1 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 455 - 558 MPa | 66000 - 81000 psi | Average value: 508 MPa Grade Count:3 |
Overview of materials for Nylon 66 Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66 Fiber". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Tensile Strength, Ultimate | >= 455 MPa | >= 66000 psi | |
Eagle Brass 19210 XP-10 Copper Iron, Extra Spring 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Strength, Ultimate | 455 - 552 MPa | 66000 - 80000 psi | |
Eagle Brass 715 Copper Nickel 30%, 1/2 Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Strength, Ultimate | 455 - 552 MPa | 66000 - 80000 psi | |
Eagle Brass 752 Nickel Silver 18%, 1/2 Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Strength, Ultimate | 455 MPa @Diameter <=15.9 mm |
66000 psi @Diameter <=0.625 in |
Rod |
CMW® 28 Copper Alloy CMW® 28 material is a copper base alloy having very high electrical and thermal conductivity and medium strength and toughness. It is a heat treatable alloy and develops its strength and hardness t.. |
|||
Tensile Strength, Ultimate | 455 MPa | 66000 psi | Drawn Rod & Bar |
CMW® 328 Copper Alloy CMW® 328 material is a high strength, high conductivity copper base alloy. CMW® 328 is heat treatable. Optimum mechanical and physical properties of CMW® 328 material are developed by heat treatm.. |
|||
Tensile Strength, Ultimate | 455 - 483 MPa | 66000 - 70100 psi | |
AK Steel 439 Ferritic Stainless steel AK Steel 439 has better oxidation and corrosion resistance than Type 409. This alloy also has optimum formability that is reproducible coil after coil and heat after heat. This provides special ad.. |
|||
Tensile Strength, Ultimate | 455 MPa @Temperature 538 °C |
66000 psi @Temperature 1000 °F |
ASTM E8 |
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 455 MPa @Temperature 204 °C |
66000 psi @Temperature 399 °F |
|
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |
|||
Tensile Strength, Ultimate | 455 MPa | 66000 psi | Typical |
Aleris Weldural Aluminum Alloy, 100 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Tensile Strength, Ultimate | 455 MPa | 66000 psi | |
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
Tensile Strength, Ultimate | 455 MPa | 66000 psi | |
PSM Industries PolyAlloys MIM-Fe-50%Ni Grade 2 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |