Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4500 MPa
653000 psi
Hexcel® IM4 Carbon Fiber (12,000 Filaments)
Weight/length = 0.723 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Tensile Strength, Ultimate 4500 MPa

@Temperature 23.0 °C
653000 psi

@Temperature 73.4 °F
AGY VeTron® Glass Fiber
Launched 2002, for Vinyl Ester and Polyester resins. Binder is VE1 silane for Vinyl Esters. Acid resistant. Moderate alkali resistance.Information provided by AGY Holding Corp.