Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 448 MPa | 65000 psi | |
Pacific Sintered Materials FCC-216-P(HT) High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | |
Pacific Sintered Materials FS-1603 Silicon Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC uses.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P(HT) Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | |
PSM Industries Pacific Sintered Metals Silicon Iron FS-1603 Powdered Metal DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC usesInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | |
Hogen Duralloy H1W 55 Tungsten/45 Copper PM Metal Composite RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is .. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | |
FloMet 304L Stainless Steel FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | |
Mi-Tech Metals CW55 55 Tungsten/45 Copper PM Metal Composite RWMA Class 10.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is recomme.. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | 1020 Steel butt joint |
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin.. |
|||
Tensile Strength, Ultimate | 448 - 552 MPa | 65000 - 80000 psi | |
Eagle Brass 725 Copper Nickel Tin, 1/2 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Strength, Ultimate | 448 - 558 MPa | 65000 - 81000 psi | |
Eagle Brass 762 Nickel Silver 12%, 1/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Strength, Ultimate | 448 MPa @Thickness <=25.0 mm |
65000 psi @Thickness <=0.984 in |
Plate |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | |
Dura-Bar 65-45-12 HRDS Continuously Cast Ductile Iron Bar Stock ASTM A536 Dura-Bar 4512 HRDS is a high-silicon ductile iron intended for use at elevated temperatures or when a part is subjected to thermal cycling, such as permanent mold applications. The ferritic structu.. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | annealed |
CMW® ELKONIUM 306 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | cold worked |
CMW® ELKONIUM 73 Copper Cadmium Alloy with Au/Ag-Cladding ELKONIUM 73 alloy is a silver, copper, cadmium and gold material marketed by CMW with high electrical and thermal properties. It is designed as an economical rivet type contact for AC applications r.. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | |
AIM 91Sn/9Zn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Tensile Strength, Ultimate | 448 MPa @Temperature 593 °C |
65000 psi @Temperature 1100 °F |
|
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | Annealed |
AK Steel 410S Ferritic Stainless steel AK Steel 410S Stainless Steel is a non-hardening modification of Type 410. A small titanium addition minimizes austenite formation at high temperatures, thereby restricting the alloy's ability to h.. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | |
Carpenter Invar 36® Alloy, Annealed Bars and Strip Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | |
ATI Allvac® 55, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Airframe skin, heat exchangers, cryogenic vessels, components for CPI equipment, condenser tubing, exhaust pipe shrouds. |
|||
Tensile Strength, Ultimate | >= 448 MPa | >= 65000 psi | |
PSM Industries PolyAlloys MIM-316L sintered Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 448 MPa | 65000 psi | ACMA Test #4 |
CeramTec 965 Toughened Alumina (Al2O3-ZrO2) Hasselman Thermal Shock value is 270 K.Data provided by CeramTec North America. |