Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 43.4 MPa | 6300 psi | ASTM D638 |
Technetics Group Amicon™ PVDF
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Tensile Strength, Ultimate | 43.4 MPa | 6300 psi | ASTM D638 |
Techmer ES Plaslube® AC-80/TF/15 Acetal (Copolymer), 15% PTFE Plaslube polytetrafluoroethylene (PTFE) lubricated acetal copolymer grades offer additional wear and friction performance over neat acetal. Typical applications include bearings, slides and small g.. |
|||
Tensile Strength, Ultimate | 43.4 MPa | 6300 psi | ASTM D638 |
American Polymers API 390 Polystyrene API 390 is a general purpose polystyrene produced in pellet form for injection molding. API 390 has excellent clarity and easy flow.Applications: Used in the manufacture of cosmetic containers, hou.. |
|||
Tensile Strength, Ultimate | 43.4 MPa | 6300 psi | ASTM D412/D638 |
Lubrizol ESTANE® 58680 Ester Based Thermoplastic Polyurethane Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 43.4 MPa | 6300 psi | |
AIM 58 Fusible Alloy Uses: lens blocking; proof casting; fusible element in safety devices; anchoring parts for machining; sealing adjustment screws; holding jet engine blades for machining and broaching; filler for sup.. |