Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 434 MPa | 62900 psi | 5% Cold Worked |
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |
|||
Tensile Strength, Ultimate | 434 MPa | 62900 psi | typical annealed |
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930 Type 409 ferritic stainless steel was introduced by Allegheny Ludlum in 1961 to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon automotive .. |