Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 38.4 MPa | 5570 psi | |
Indium Corp. Indalloy® 233 Pb-Sb-Sn Solder Alloy Intermediate temp solder. Creep resistant.Information provided by the manufacturer, Indium Corporation. |