Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 379 MPa | >= 55000 psi | |
PSM Industries PolyAlloys MIM-2700 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | >= 379 MPa | >= 55000 psi | |
PSM Industries PolyAlloys MIM-4605 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 379 MPa | 55000 psi | |
FloMet 430L Stainless Steel FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Ultimate | 379 - 414 MPa | 55000 - 60000 psi | |
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 379 MPa | 55000 psi | Armco Iron (0.05% C) butt joint |
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin.. |
|||
Tensile Strength, Ultimate | 379 MPa @Temperature 760 °C |
55000 psi @Temperature 1400 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Ultimate | 379 MPa @Temperature 760 °C |
55000 psi @Temperature 1400 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Ultimate | >= 379 MPa | >= 55000 psi | |
Alcoa Excalibar® 6013-T651 Aluminum Alcoa recommends as a higher machinability alternative to 6061-T651. It has the potential for higher machining speeds and feed rates, easier deburring,ease of clearing 'chips' and better finishes. .. |
|||
Tensile Strength, Ultimate | 379 - 448 MPa | 55000 - 65000 psi | |
Eagle Brass 240 Low Brass, 1/2 Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Ultimate | 379 - 483 MPa | 55000 - 70000 psi | |
Eagle Brass 511 Phosphor Bronzes 4%, 1/2 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Ultimate | 379 - 517 MPa | 55000 - 75000 psi | |
Eagle Brass 725 Copper Nickel Tin, 1/4 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Strength, Ultimate | 379 - 455 MPa @Thickness 1.27 - 2.16 mm |
55000 - 66000 psi @Thickness 0.0500 - 0.0850 in |
Annealed, Transverse Orientation |
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |
|||
Tensile Strength, Ultimate | 379 - 482 MPa | 55000 - 69900 psi | |
Ametek AM 388™ Alloy (UNS C72650) TB00 Solution HT Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Ultimate | 379 - 483 MPa | 55000 - 70100 psi | |
Ametek High Purity Nickel Strip 899A 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 379 - 483 MPa | 55000 - 70100 psi | |
Ametek High Purity Nickel Strip 899L 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 379 - 483 MPa | 55000 - 70100 psi | |
Ametek High Purity Nickel Strip 899M 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 379 MPa @Temperature 649 °C |
55000 psi @Temperature 1200 °F |
ASTM E8 |
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 379 MPa | 55000 psi | |
AIM 58Bi/42Sn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Tensile Strength, Ultimate | >= 379 MPa | >= 55000 psi | Minimum; longitudinal direction. (Transverse values generally lower). |
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |
|||
Tensile Strength, Ultimate | >= 379 MPa | >= 55000 psi | Minimum |
Materion AlBeMet® AM 162 Rolled Sheet, Annealed Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are.. |