Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D638 |
Multibase Nylex™ 2185 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D638 |
Rostone Rosite® C200BS ESD SMC, Conductive Thermoset Polyester, 10% Glass Reinforced
(discontinued **) Key Features: Electrostatic DissipativeRosite Conductive C used in applications such as molded paper guides in printers and plotters. Conductive C is the UL recognition.Information provided by Onei.. |
|||
Tensile Strength, Ultimate | 37.3 MPa | 5400 psi | DIN 53455; ASTM D638 |
Kolon KOPEL® KP3363 General Purpose TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | |
Indium Corp. Indalloy® 117 Bi-Pb-In-Sn-Cd Fusible Alloy General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Tensile Strength, Ultimate | 37.3 MPa | 5400 psi | ASTM D412 |
SK Chemicals SKYTHANE® CS195A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 37.3 MPa | 5400 psi | ASTM D412 |
SK Chemicals SKYTHANE® S195A C series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 37.3 MPa | 5400 psi | ASTM D412 |
SK Chemicals SKYTHANE® 470A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | |
Williams Advanced Alloys WS238 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D638 |
Total PPH 3620WZ Polypropylene, Injection Molding Grade Injection molding homopolymerNucleation - FINA 3620WZ is engineered with nucleation to provide fast cycle time and improve contact clarity in thin wall multi- cavity molds.Antistat - FINA 3620WZ con.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D412/D638 |
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane Features: Good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion.Available in Americas, Europe, Midd.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D412 |
Lubrizol Estane® 5712 Thermoplastic Polyurethane Type: Estane® 5712 is a Polyester thermoplastic polyurethane (TPU).Feature: It has the highest peel and green strengths and shortest open-tack time of any Estane TPU resin used in adhesives. Suppl.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D638 |
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D638 |
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions .. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D638 |
Buckeye Polymers BP ABS 6432 WS ABS ABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processing and outs.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | |
BCC Products BC 7009-2 Epoxy Casting BC 7009-2 is an iron filled, low-cost mass casting system. Recommended for use in casting a minimum of two inches and a maximum of six inches in non-conductive molds. Thicknesses to nine inches in m.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | |
AIM 47 Fusible Bismuth Alloy Uses: low-temperature solder; fixturing delicate parts for machining; lens blocking; proof casting of cavities; dental models; fusible element in safety devices and alarms; radiation blocking for x-.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D412 |
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Memory, elasticity and impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane prod.. |
|||
Tensile Strength, Ultimate | 37.2 MPa | 5400 psi | ASTM D638-95 |
Multibase Multi-ABS 3075 High Impact Data provided by Multibase. |