Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 36.5 MPa | 5300 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AS-10GB/02S Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **)< Description/Features:Glass Bead FilledSilicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 36.5 - 55.2 MPa | 5300 - 8000 psi | Average value: 48.1 MPa Grade Count:7 |
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Thermoplastic Polyurethane Blend". Each property range of values reported is minimum and m.. |
|||
Tensile Strength, Ultimate | 36.5 - 241 MPa | 5300 - 35000 psi | Average value: 174 MPa Grade Count:7 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Ultimate | 36.5 - 200 MPa | 5300 - 29000 psi | Average value: 147 MPa Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Tensile Strength, Ultimate | 36.5 MPa | 5300 psi | ASTM D638 |
Techmer ES Electrafil® DB-1200/S/7/FR ABS, 7% Stainless Steel Fiber Reinforced (dry blend), Flame Retardant Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL.. |
|||
Tensile Strength, Ultimate | 36.5 MPa | 5300 psi | |
Williams Advanced Alloys WS205 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 36.5 MPa | 5300 psi | ASTM D412 |
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el.. |
|||
Tensile Strength, Ultimate | 36.5 MPa | 5300 psi | ASTM D638 |
American Polymers API 500 Polystyrene API 500 is a heat resistant grade of impact polystyrene. It has superior heat resistance, good impact resistance and easy colorability.Applications: API 500 is used in housewares, toys, containers,.. |
|||
Tensile Strength, Ultimate | 36.5 MPa | 5300 psi | ASTM D412 |
Lubrizol Estane® ALR PC73A Thermoplastic Polyurethane Type: Estane® ALR PC73A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |
|||
Tensile Strength, Ultimate | 36.5 MPa | 5300 psi | after optimum cure |
Armstrong A-1/A Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Tensile Strength, Ultimate | 36.5 MPa | 5300 psi | |
BCC Products BC 7062H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |