Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 36.5 - 44.1 MPa | 5290 - 6400 psi | ASTM D638 |
Novatec Novacycle® 501 PVC Novacycle® 501 is a general purpose, rigid, extrusion grade PVC compound in pellet form. This formulation is designed to provide an economical alternative for extruded profiles Raw material appe.. |
|||
Tensile Strength, Ultimate | 36.5 MPa @Temperature 300 °C |
5290 psi @Temperature 572 °F |
ASTM D638 |
Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Tensile Strength, Ultimate | 36.5 MPa | 5290 psi | ASTM D638 |
DuPont™ Surlyn® 9120 Ionomer Resin, Zinc Surlyn® 9120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Tensile Strength, Ultimate | 36.5 MPa | 5290 psi | ASTM D638 |
Eastman Tenite Propionate 358A4000008 Clear, Trsp Cellulose Acetate Propionate Plasticizer 14%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |