Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 359 MPa | 52000 psi | |
Pacific Sintered Materials SS-316-SH 316L Stainless Steel Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 359 MPa | 52000 psi | |
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-SH Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 359 MPa | 52000 psi | Longitudinal |
Special Metals Electroformed Nickel, 200 Micron (8 mil) Foil, Electroformed and Annealed Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | >= 359 MPa | >= 52000 psi | |
Eagle Brass 110 EPT COPPER, Extra Spring Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Ultimate | 359 - 448 MPa | 52000 - 65000 psi | |
Eagle Brass 18665 MSP1, 1/4 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Strength, Ultimate | 359 - 427 MPa | 52000 - 62000 psi | |
Eagle Brass 19210 XP-10 Copper Iron, 3/4 Hard 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Strength, Ultimate | 359 - 427 MPa | 52000 - 62000 psi | |
Eagle Brass 220 Commercial Bronze, 3/4 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Strength, Ultimate | >= 359 MPa | >= 52000 psi | |
Eagle Brass 715 Copper Nickel 30%, Annealed 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Strength, Ultimate | 359 MPa @Temperature 482 °C |
52000 psi @Temperature 900 °F |
|
Dura-Bar 65-45-12 HRDS Continuously Cast Ductile Iron Bar Stock ASTM A536 Dura-Bar 4512 HRDS is a high-silicon ductile iron intended for use at elevated temperatures or when a part is subjected to thermal cycling, such as permanent mold applications. The ferritic structu.. |
|||
Tensile Strength, Ultimate | >= 359 MPa | >= 52000 psi | |
Eagle Brass 101 OFE COPPER (Certified), Extra Spring Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Ultimate | >= 359 MPa | >= 52000 psi | |
Eagle Brass 102 OF COPPER (Non-Certified), Extra Spring Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |