Tensile Strength, Ultimate 353 MPa
51200 psi
Pacific Sintered Materials FP-1650-S Phosphorous Iron Soft Magnetic Powdered Metal
For applications requiring high yield strength and toughness. Magnetic properties superior to iron, but slightly inferior to silicon iron.All information provided by Pacific Sintered Metals.
Tensile Strength, Ultimate 353 MPa
51200 psi
PSM Industries Pacific Sintered Metals Phosphorous Iron FP-1650-S Powdered Metal
For applications requiring high yield strength and toughness. Magnetic properties superior to iron, but slightly inferior to silicon iron.Information Provided by Pacific Sintered Metals, a division ..