Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3.50 MPa | 508 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 7020 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 3.50 MPa @Temperature 800 °C |
508 psi @Temperature 1470 °F |
|
Pyrotek U-1 Compressible Board U-1 is a high-temperature millboard that is easily cut, punched and shaped. It works well as a roll-cladding material and as compressible gasketing. A unique characteristic of the asbestos-free bo.. |