Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Pacific Sintered Materials FCC-216-P High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
PSM Industries Pacific Sintered Metals Nickel Steel FN-255-S Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0205-25Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed Nominal Composition: Ti-0.4 Ni-0.015 Pd-0.025 Ru-0.14 Cr Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant... |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
Kobe Steel KSTI-1.5AL Alpha Titanium Alloy, Annealed Nominal Composition: Ti-1.5 Al Applications: Exhaust systems.Features:Heat resistant. Information provided by Kobe Steel |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
Kobe Steel Titanium alloy with low alloying elements, ASTM Gr. 7, Annealed Nominal Composition: Ti-0.15 Pd Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by .. |
|||
Tensile Strength, Ultimate | 345 - 517 MPa | 50000 - 75000 psi | |
Materion ToughMet® T3 CA ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Ultimate | 345 - 414 MPa | 50000 - 60000 psi | |
Meehanite Almanite® W2 Wear and Abrasion Resisting Cast Iron Type W2 is an austenitic-martensitic white iron characterized by high hardness and relatively good impact strength. Type W2 has a martensitic matrix.General Meehanite information - Meehanite metal .. |
|||
Tensile Strength, Ultimate | 345 - 448 MPa | 50000 - 65000 psi | |
Meehanite AQ Flake Graphite Cast Iron Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treate.. |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
MetalTek MTEK CZ-100 Cast UNS N02100 Severe Corrosion and Heat Resistant Alloy Strong, tough and resistant to a wide range of industrial chemicals.Applications: Process equipment; food, pharmaceutical and chemical.Information provided by MetalTek |
|||
Tensile Strength, Ultimate | 345 MPa @Temperature 870 °C |
50000 psi @Temperature 1600 °F |
|
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | Annealed |
Special Metals Nickel 205 Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | Annealed |
Special Metals Nickel 270 A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Universal Wire Works 187 Copper-Nickel Alloy Welding Wire Alloy 187 is used for arc welding of wrought or cast 70/30, 80/20, and 90/10 copper nickel alloys to themselves or to each other. Alloy 187 can be used for welding the clad side of copper-nickel cla.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Universal Wire Works Commercially Pure (AMS 4951) Titanium Alloy Filler Metal Universal commercially pure titanium is extremely versatile for applications requiring high temperature resistance together with resistance to many chemical reagents. Commercially pure (cp) titanium.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Eagle Brass 110 EPT COPPER, Spring Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Ultimate | 345 - 407 MPa | 50000 - 59000 psi | |
Eagle Brass 210 Gilding Metal, Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Ultimate | 345 - 469 MPa | 50000 - 68000 psi | |
Eagle Brass 735 Nickel Silver 18%, Annealed 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | Premium Casting |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | cold worked |
CMW® D50F Silver Nickel Alloy CMW® D50F can be fabricated into wire, rod and strip; however, the headability of CMW® D50F is limited to a narrow range. It is used for main contacts in circuit breakers and switching devices whe.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | cold worked |
CMW® ELKONIUM 23 silver, copper alloy Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Eagle Brass 101 OFE COPPER (Certified), Spring Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Eagle Brass 102 OF COPPER (Non-Certified), Spring Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | cold worked |
CMW® ELKONIUM 63 Silver Alloy ELKONIUM® 63 alloy contains small amounts of magnesium and nickel. It is recommended for low voltage, vibrating contact DC applications for minimizing metal transfer. It is used in automobile volta.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (FS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Ametek High Purity Nickel Strip 899L Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Ametek P316L P/M Stainless Steel, Sintered from 6.30 g/cc Green Density P316L offers a very high degree of corrosion protection for a standard P/M stainless steel grade. It provides excellent strength at extremely high temperatures. Key materials benefits of P316L inclu.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
ATI Allegheny Ludlum Grade 17 Titanium (UNS R52252) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (CS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
ATI Allvac® 40, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets. |