Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM D412 |
MF-5062 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | TM R050-36 |
Resinlab® SEC1244 Silver Filled Epoxy Adhesive Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth.. |
|||
Tensile Strength, Ultimate | 34.5 - 74.0 MPa | 5000 - 10700 psi | Average value: 54.2 MPa Grade Count:7 |
Overview of materials for Polyphenylene Ether, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | 34.5 - 91.0 MPa | 5000 - 13200 psi | Average value: 58.1 MPa Grade Count:23 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Ultimate | 34.5 - 44.8 MPa | 5000 - 6500 psi | Average value: 39.5 MPa Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PE-40MC/000 High Density Polyethylene (HDPE)
(discontinued **) Description/Features:Mica FilledInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | ASTM D638 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | |
Indium Corp. Indalloy® 206 Pb-In Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | Machine direction |
Spartech Centrex® R83/21 ABS Weather Resistant Sheet Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM Data |
Styron Magnum™ 275 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM Data |
Styron Magnum™ 8325 ABS, Sheet Coextrusion Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM Data |
Styron Magnum™ 9085 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM Data |
Styron Magnum™ 9095 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM Data |
Styron Magnum™ 9450P ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM Data |
Styron Magnum™ 213 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | |
Williams Advanced Alloys WS257 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM D412 |
Lubrizol Estane® MVT 90AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 90AF3 TPU is a 90A aromatic polyether-based thermoplastic polyurethane.Features: High moisture vapor transmission, good physical properties and elasticity, free of organo-tin comp.. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM D638 |
Ecomass® 1050TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Techn.. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM D638 |
Ecomass® 1066ZD96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM D638 |
Buckeye Polymers BP ABS 7626 ABS High ImpactABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processi.. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium .. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Tensile Strength, Ultimate | 34.5 MPa @Temperature 871 °C |
5000 psi @Temperature 1600 °F |
|
ATI Allegheny Ludlum AL 468™ Dual Stabilized- Low Titanium Stainless Steel Characteristics:good corrosion resistance in a wide range of environments, can be used in annealed cold formed or as-welded conditions. Applications: used in place of Type 304 in an oxidizing when .. |
|||
Tensile Strength, Ultimate | 34.5 - 68.9 MPa | 5000 - 10000 psi | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |