Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 344 MPa | 49900 psi | ASTM D638 |
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC QC-8800 is a vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested for ap.. |
|||
Tensile Strength, Ultimate | 344 - 413 MPa | 49900 - 59900 psi | |
Kennametal Stellite Stellite® 33 Completely non-magnetic. Specific Electrical Resistance: 39.8 µOhm/in^3.Applications: standard tool bits, tipped tools, form tools, milling cutter blades, wood working tools, reamer blades, cut-o.. |
|||
Tensile Strength, Ultimate | 344 MPa | 49900 psi | ASTM D638 |
Quantum Composites QC-8770 63% Glass Fiber Hybrid Vinyl Ester SMC
(discontinued **) QC-8770 is a hybrid vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and excellent st.. |