Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 338 MPa

@Temperature 260 °C
49000 psi

@Temperature 500 °F
Stainless Steel (18-8) butt joint
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin..
Tensile Strength, Ultimate 338 - 407 MPa
49000 - 59000 psi
Eagle Brass 260 Cartridge Brass, 1/4 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Tensile Strength, Ultimate 338 - 421 MPa
49000 - 61000 psi
Eagle Brass 510 Phosphor Bronzes 5% A, 1/4 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Ultimate 338 MPa

@Temperature 538 °C
49000 psi

@Temperature 1000 °F
AK Steel 18 SR® Ferritic Stainless steel
AK Steel 18 SR® provides excellent resistance to high temperature scaling - far superior to that of Type 446 stainless steel. This material is readily welded by conventional methods. It is not su..
Tensile Strength, Ultimate 338 MPa
49000 psi
AK Steel Aluminized Carbon Steel, Deep Drawing Steel (DDS Type B), Standard Grade
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. DDS is made by adding aluminum to the molten steel and..