Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 317 MPa
46000 psi
PSM Industries Pacific Sintered Metals Bronze BT-126 Powdered Metal
Higher strength structural and bearing bronzeInformation Provided by Pacific Sintered Metals, a division of PSM Industries
Tensile Strength, Ultimate 317 - 386 MPa
46000 - 56000 psi
Eagle Brass 210 Gilding Metal, 3/4 Hard
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi..
Tensile Strength, Ultimate 317 - 386 MPa
46000 - 56000 psi
Eagle Brass 510 Phosphor Bronzes 5% A, Annealed
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Ultimate 317 - 400 MPa
46000 - 58000 psi
Eagle Brass 511 Phosphor Bronzes 4%, 1/4 Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
Tensile Strength, Ultimate 317 - 372 MPa
46000 - 54000 psi
Eagle Brass 511 Phosphor Bronzes 4%, Annealed
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
Tensile Strength, Ultimate 317 MPa
46000 psi
Worked
CMW® D54F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3
For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc.
Tensile Strength, Ultimate 317 MPa
46000 psi
AK Steel Cold Rolled Carbon Steel, Commercial Steel (CS Type B), Standard Grade
May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel
Tensile Strength, Ultimate 317 MPa
46000 psi
.0275 - .035 inches sheet thickness; ASTM A 370
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade
Interstitial Free (I-F) steels are made by adding titanium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel
Tensile Strength, Ultimate 317 MPa
46000 psi
.0275 - .035 inches sheet thickness; ASTM A 370
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Deep Drawing Steel (DDS Type B), Standard Grade
DDS may be used in drawing applications.Information provided by AK Steel
Tensile Strength, Ultimate 317 MPa
46000 psi
AIM 62Sn/Pb36/Ag2 Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Tensile Strength, Ultimate 317 MPa
46000 psi
.0275 - .035 inches sheet thickness; ASTM A 370
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Drawing Steel (DS Type B), Standard Grade
DS Type B may be used in drawing applications.Information provided by AK Steel
Tensile Strength, Ultimate 317 MPa
46000 psi
Pacific Sintered Materials BT-126 Bronze Powdered Metal
Applications: Higher strength structural and bearing bronze.All information provided by Pacific Sintered Metals.