Polymer Property : Tensile Strength, Ultimate = 4220 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 29.1 MPa
4220 psi
ASTM D638
NOVA Chemicals Novapol® TI-0338-A MDPE Masterbatch Resin
Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer.
Tensile Strength, Ultimate 29.1 MPa
4220 psi
ASTM D638
NOVA Chemicals Novapol® TR-0338-U MDPE Rotational Molding Resin  (discontinued **)
Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer.
Tensile Strength, Ultimate 29.1 MPa
4220 psi
Vulcanized
KKPC KOSYN 1500M Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tensile Strength, Ultimate 29.1 MPa
4220 psi
Vulcanized
KKPC KOSYN 1502W Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tensile Strength, Ultimate 29.1 MPa
4220 psi
150°C, 40 min., Pressure Vulcanization. -10% Change after 100°C, 70 hrs, Oil Immersion
KKPC KOSYN KNB 25H Acrylonitrile Butadiene Rubber (NBR)
Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. ..
Tensile Strength, Ultimate 29.1 MPa
4220 psi
ASTM D638
NOVA Chemicals Novapol® TR-0338-UG MDPE Rotational Molding Resin  (discontinued **)
Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer.