Polymer Property : Tensile Strength, Ultimate = 39000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 269 - 324 MPa
39000 - 47000 psi
Eagle Brass 230 Red Brass, Annealed
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Tensile Strength, Ultimate 269 MPa

@Temperature 538 °C
39000 psi

@Temperature 1000 °F
Crucible Steel 430 Chromium Steel
Crucible 430 is essentially a non-hardenable chromium steel which is adaptable for general purpose corrosion and heat resisting applications. It is prone to slight hardening by heat treatment. This..
Tensile Strength, Ultimate 269 MPa
39000 psi
Annealed
CMW® D54F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3
For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc.
Tensile Strength, Ultimate 269 MPa
39000 psi
Worked
CMW® D55X Post-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3
For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc.