Polymer Property : Tensile Strength, Ultimate = 363 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.50 MPa
363 psi
Momentive Performance Materials RTV5242 White Adhesive Sealant, Fast Cure Paste
One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Fast cure, true neu..
Tensile Strength, Ultimate 2.50 MPa
363 psi
Momentive Performance Materials RTV5249 Gray Adhesive Sealant, Fast Cure Paste
One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Fast cure, true neu..
Tensile Strength, Ultimate >= 2.50 MPa
>= 363 psi
ASTM D412
Multibase Multi-Flex® TPE A 4710 BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tensile Strength, Ultimate 2.50 MPa
363 psi
Momentive Performance Materials RTV5243 Black Adhesive Sealant, Fast Cure Paste
One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Fast cure, true neu..
Tensile Strength, Ultimate 2.50 MPa
363 psi
Dow Corning 7091 ADHESIVE SEALANT
High performance, neutral cure silicone adhesive/sealant.Information provided by Dow Corning
Tensile Strength, Ultimate 2.50 MPa
363 psi
Foaming Direction
Cymat A35620SC 030SS Stabilized Aluminum Foam
Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it ..