Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.45 MPa | 355 psi | |
Momentive Performance Materials RTV116 Red Adhesive Sealant, High Temperature Pourable One-part alkoxy cure. Typical uses: High-heat applications; encapsulate and seal heating elements.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance.. |
|||
Tensile Strength, Ultimate | 2.45 MPa | 355 psi | |
Momentive Performance Materials RTV8111 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |