Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.41 MPa | 349 psi | |
Valley Adhesives EM-105 High Performance Application Glue Stick Valley Adhesives EM-105 High Performance Application Glue StickHigh peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, pol.. |