Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2400 MPa | 348000 psi | |
Cytec Thornel® P-100 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction.0.32 m/g yield, 0 or 32 tpm t.. |
|||
Tensile Strength, Ultimate | 2400 MPa | 348000 psi | |
Cytec Thornel® P-120 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction.2000 filaments/strand, 0.33 m.. |
|||
Tensile Strength, Ultimate | 2400 MPa | 348000 psi | |
China Tungsten YG11 Tungsten Carbide Powder Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 2400 MPa | 348000 psi | |
China Tungsten YG13X Tungsten Carbide Powder Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 2400 MPa | 348000 psi | |
China Tungsten YG25C Tungsten Carbide Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 2400 MPa | 348000 psi | |
China Tungsten YG9C Tungsten Carbide Powder Information provided by China Tungsten |