Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 22.4 MPa | 3250 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO D 5302 E MB Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 22.4 MPa | 3250 psi | |
Sylvin Technologies 9604-80C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 22.4 - 200 MPa @Temperature -40.0 - 150 °C |
3250 - 29000 psi @Temperature -40.0 - 302 °F |
Average value: 87.1 MPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Tensile Strength, Ultimate | 22.4 - 200 MPa @Strain 0.140 - 4.69 % |
3250 - 29000 psi @Strain 0.140 - 4.69 % |
Average value: 87.1 MPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Tensile Strength, Ultimate | 22.4 MPa | 3250 psi | ASTM D412 |
PB1100-75 Polyurethane-based Biomedical Elastomer |