Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1970 MPa | 285000 psi | |
Latrobe Lescalloy® 35NCD16 VAC-ARC High Strength Alloy Steel LESCALLOY 35NCD16 VAC-ARC is a high strength, low alloy vacuum arc remelted steel which takes its name from the French industry designation. The combination of high strength, high fracture toughnes.. |
|||
Tensile Strength, Ultimate | 1965 MPa | 285000 psi | |
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 482°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |
|||
Tensile Strength, Ultimate | 1970 MPa | 285000 psi | Oil Quenched from 871°C; 204°C Temper Temperature |
Latrobe Staminal™ Shock Resisting Die Steel Staminal is an air or oil hardening die steel containing a large percentage of nickel combined with a proper balance of other alloying elements for deep hardening and extreme toughness. For tools, .. |