Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1900 MPa | 276000 psi | 204°C Temper Temperature |
Latrobe Lescalloy® 4340 VAC-ARC ; 3.5" round High Strength Alloy Steel LESCALLOY 4340 VAC-ARC steel is a low alloy, nickel-chromium-molybdenum steel capable of being heat treated to high strength levels. The alloy has a good combination of ductility, toughness and str.. |
|||
Tensile Strength, Ultimate | 1900 MPa | 276000 psi | |
Cytec Thornel® P-55S 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, high modulus strands made from a pitch precursor. The fiber surface has been treated to increase the interla.. |
|||
Tensile Strength, Ultimate | 1900 MPa | 276000 psi | |
Cytec Thornel® P-75S 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus strands made from a pitch precursor. The fiber surface has been treated to increase the i.. |
|||
Tensile Strength, Ultimate | 1900 MPa | 276000 psi | |
AIM 80Au/20Sn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Tensile Strength, Ultimate | 1900 MPa @Temperature 23.0 °C |
276000 psi @Temperature 73.4 °F |
|
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |