Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1830 MPa | 265000 psi | 50% Cold Rolled (4 hrs at 1025°F/550°C) |
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
Tensile Strength, Ultimate | 1830 MPa | 265000 psi | 260°C Temper Temperature |
Latrobe Lescalloy® 4340 VAC-ARC ; 7.5" square High Strength Alloy Steel LESCALLOY 4340 VAC-ARC steel is a low alloy, nickel-chromium-molybdenum steel capable of being heat treated to high strength levels. The alloy has a good combination of ductility, toughness and str.. |
|||
Tensile Strength, Ultimate | 1830 MPa | 265000 psi | Precipitation Hardened |
Special Metals UDIMET® Alloy 250 Maraging Steel A high-strength, maraging steel of iron and nickel with additions of molybdenum and titanium. It has the strength of standard 18Ni (250) maraging steel but the advantages of containing less molybde.. |
|||
Tensile Strength, Ultimate | 1830 MPa | 265000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Tensile Strength, Ultimate | 1827 MPa | 265000 psi | |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition CH 900 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Tensile Strength, Ultimate | 1827 MPa | 265000 psi | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 55% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |