Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.172 - 86.6 MPa | 25.0 - 12600 psi | Average value: 23.7 MPa Grade Count:20 |
Overview of materials for Epoxy Adhesive, Flexible This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro.. |
|||
Tensile Strength, Ultimate | 0.172 MPa | 25.0 psi | cured 7 days @ 25°C |
Abatron AboCast/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |