Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Tensile Strength, Ultimate | 15.9 - 34.5 MPa | 2310 - 5000 psi | Average value: 28.3 MPa Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | ASTM D638 |
DuPont™ Surlyn® 9320W Ionomer Resin, Zinc
(discontinued **) Surlyn® 9320W thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. This very low modulus zinc.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | |
Freudenberg Simrit N470 Hydrocarbon Elastomer Nitrile Standard Nitrile is also known as Buna-N. Excelent resistance to petroleum-based oils and fuels, water and alcohols. Nitrile also has good resistance to acids and bases, except those with a strong o.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | ASTM Data |
Dow AIM® 4900 High Impact Styrenic Resin AIM® 4900 advanced styrenic resin for extrusion and thermoforming applications is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | Molded property |
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | Vulcanizate, Press cured, TC95 +3min at 180°C |
Dow Nordel® IP 5565 Heat Resistant Peroxide Cured FormulationNordel® IP 5565 |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | ASTM D638 |
Buckeye Polymers BP Flex D6707 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | 10 in/min; ASTM D412 |
PolyOne Elastamax XL-0257-2 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color.. |