Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 8980-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 8999-95 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 9604-80 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 9812A-95 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 9925-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 5108 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Cytec EN-7 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Cytec EN-8 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D-638 |
CMT Materials REN Shape® 450 Prototype Tool & Modeling Board REN Shape 450 is the preferred modeling board for pattern makers throughout the world. The outstanding dimensional stability and its ability to hold precise tolerances even after exposure to heat h.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D412 |
Colorite Polymers CS8039UL Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D412 |
Colorite Polymers CS9040UL--85B Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D412 |
Colorite Polymers Weatherflex™ CS1536WX (NTL70B) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D638 |
Colorite Polymers 7077 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D638 |
Colorite Polymers 7444D General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D638 |
Colorite Polymers 7500 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Colorite Polymers 7812 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D638 |
Colorite Polymers 8090C General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D412 |
Colorite Polymers CS1537SC Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Dymax 3093 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Colorite Polymers Self Frosting™ 7811SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Dymax 625 Structural Adhesive Structural Adhesives for Rugged Bonding, Sealing, Tacking and Potting in SecondsMulti-Cure® 600 Series products are rapid setting adhesives that cure by UV light, activator or heat. These products .. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D638 |
Colorite Polymers 7002A-02 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D412 |
BCC Products BC 8675E Polyurethane Elastomer BC 8675E is a multi-purpose elastomer that can perform many functions. Typical product features are: easy to use, cures at room temperature, resists moisture absorption, excellent in use for molds f.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 6147-83 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 6148-90 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 9604-95 LMW Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Colorite Polymers 7811 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |