Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.150 - 51.0 MPa | 21.8 - 7400 psi | Average value: 27.7 MPa Grade Count:22 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |