Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 14.1 MPa | 2050 psi | |
Sylvin Technologies 8600-70 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 14.1 MPa | 2050 psi | |
Sylvin Technologies 9600-70 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 14.1 MPa | 2050 psi | 10 in/min; ASTM D412 |
PolyOne Elastamax XL 0254-15 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a urethane based thermoplastic elastomer specially lubricated for auto suspension bushings. Physical Form: Pellets. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hann.. |