Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1400 - 1430 MPa | 203000 - 208000 psi | |
Latrobe Lescalloy® UT-18 VAC-ARC ; 2.125 in. round High Strength Alloy Steel UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting.. |
|||
Tensile Strength, Ultimate | 1400 - 1410 MPa | 203000 - 204000 psi | |
Latrobe Lescalloy® UT-18 VAC-ARC ; 3.75 in. round High Strength Alloy Steel UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting.. |
|||
Tensile Strength, Ultimate | 1400 - 1600 MPa | 203000 - 232000 psi | |
SSAB Tunnplat Docol® 1400 DP High-strength Steel The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel .. |
|||
Tensile Strength, Ultimate | 1400 MPa | 203000 psi | Filament Property. Mat strength is 120 N/m |
Cytec Thornel® Mat VMA Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Composed of high strength, high modulus carbon filaments in a random-layered orientation. The fine diameter filaments are up to th.. |
|||
Tensile Strength, Ultimate | 1400 MPa | 203000 psi | Filament Property. Mat strength is 120 N/m |
Cytec Thornel® Mat VMC Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Prepared by sectioning mat VMA into cubes ~ 0.5x0.5x1.0 in. VMC can be heterogeneously dispersed in matrix materials and thus enha.. |
|||
Tensile Strength, Ultimate | 1400 MPa | 203000 psi | Filament Property. Mat strength is 120 N/m |
Cytec Thornel® Mat VMD Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 400 µm - adequate for good property improvement... |
|||
Tensile Strength, Ultimate | 1400 MPa | 203000 psi | Filament Property. Mat strength is 120 N/m |
Cytec Thornel® Mat VME Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 200 µm - inadequate for good mechanical property.. |
|||
Tensile Strength, Ultimate | 1400 MPa | 203000 psi | |
Cytec Thornel® P-25 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament strand from a pitch precursor.2000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 3.1 m/g yield.. |
|||
Tensile Strength, Ultimate | 1400 MPa | 203000 psi | |
Cytec Thornel® P-25 4K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament strand from a pitch precursor.4000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 1.4 m/g yield.. |
|||
Tensile Strength, Ultimate | 1400 MPa | 203000 psi | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |