Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1284 MPa @Treatment Temp. 593 °C, Time 2.88e+7 sec |
186200 psi @Treatment Temp. 1100 °F, Time 8000 hour |
Room temp test after thermal exposure |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |