Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1240 - 1520 MPa | 180000 - 220000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Ultimate | >= 1241 MPa | >= 180000 psi | |
Kobe Steel KS15-3-3-3 Beta Titanium Alloy, AMS 4914, Solution treated and aged 482°C, 16 hrs - AC Nominal Composition: Ti-15 V-3 Cr-3 Sn-3 AlApplications: Aircraft parts, bicycle gears, gold club heads, foils. Features:Super high strength.Information provided by Kobe Steel |
|||
Tensile Strength, Ultimate | 1240 - 1520 MPa | 180000 - 220000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Ultimate | 1240 - 1520 MPa | 180000 - 220000 psi | |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; over 9.5 to 25.4 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Ultimate | 1240 - 1520 MPa | 180000 - 220000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Ultimate | 1240 - 1340 MPa | 180000 - 195000 psi | |
Materion BrushCAST® 275CT Fine Grain Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Ultimate | 1240 MPa | 180000 psi | A+ age at 975°C for 20 hours |
Latrobe Nitralloy® N™ VAC-ARC Premium Nitriding Steel NITRALLOY N is an age hardenable nitriding steel. The age hardening capability of the alloy permits the core strength to be developed while the surface is being nitrided. VAC-ARC remelting is employ.. |
|||
Tensile Strength, Ultimate | 1241 - 1413 MPa | 180000 - 204900 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH4, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Ultimate | 1240 - 1340 MPa | 180000 - 195000 psi | |
Materion BrushCAST® 275C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Ultimate | 1240 MPa | 180000 psi | |
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Ultimate | 1241 MPa | 180000 psi | |
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 1 hour at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Ultimate | >= 1241 MPa | >= 180000 psi | |
HP Alloys Nitronic® 50 Austenitic Stainless, Level 4 Cold Worked Cold Worked applies to tensile values and are for 1/4 to 2 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resist.. |
|||
Tensile Strength, Ultimate | 1240 - 1590 MPa | 180000 - 230000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the .. |
|||
Tensile Strength, Ultimate | 1240 MPa | 180000 psi | Same value for longitudinal and transverse |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D.. |
|||
Tensile Strength, Ultimate | >= 1240 MPa | >= 180000 psi | |
Special Metals Nitinol Body-Temperature Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Tensile Strength, Ultimate | >= 1240 MPa | >= 180000 psi | |
Special Metals Nitinol High-Temperature Shape Memory Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Tensile Strength, Ultimate | 1240 MPa | 180000 psi | |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®.. |
|||
Tensile Strength, Ultimate | 1241 MPa @Temperature -253 °C |
180000 psi @Temperature -423 °F |
Transverse |
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Ultimate | 1241 MPa | 180000 psi | |
ATI Allvac® 706 Nickel Superalloy, Heat Treatment: 954°C (1750°F) + Age Data provided by Allvac.Applications: Land based turbine wheels and spacers. Jet engine components. |
|||
Tensile Strength, Ultimate | 1241 MPa | 180000 psi | |
ATI Allvac® Astroloy Nickel Superalloy, Heat Treatment: 1163°C (2125°F) + Age Data provided by Allvac.Applications: Discs, rings, bolts for gas turbines. |
|||
Tensile Strength, Ultimate | 1241 MPa | 180000 psi | |
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age Data provided by Allvac.Applications: Jet and rocket engines, torque rings, afterburners, and hardware; space shuttle turbo pumps seals. |
|||
Tensile Strength, Ultimate | 1241 MPa @Temperature 427 °C |
180000 psi @Temperature 801 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Tensile Strength, Ultimate | 1241 MPa @Temperature -73.0 °C |
180000 psi @Temperature -99.4 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 20% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
Tensile Strength, Ultimate | 1241 MPa | 180000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 60% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Ultimate | 1241 MPa @Temperature -73.0 °C |
180000 psi @Temperature -99.4 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Ultimate | >= 1240 MPa | >= 180000 psi | |
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated plus Precipitation Heat Treated, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |
|||
Tensile Strength, Ultimate | >= 1241 MPa | >= 180000 psi | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 4 Cold Worked Level 4 Cold Worked applies to tensile properties of 0.25 to 2 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin.. |