Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1210 MPa | 175000 psi | |
Kinetics MIM 17-4PH Stainless Steel (H900 Condition) Precipitation-hardening stainless steel. Offers a good balance between corrosion resistance and strength. Magnetic. Hardenable to various strength levels and hardness by varying the aging heat treat.. |
|||
Tensile Strength, Ultimate | 1210 MPa | 175000 psi | |
Meehanite K-405 Austempered Ductile Iron Type K-405 is for applications involving wear and requiring high tensile and endurance limit. Excellent founding properties enable more accurate castings with savings in machine stock required. Da.. |
|||
Tensile Strength, Ultimate | >= 1210 MPa | >= 175000 psi | H1050 Condition - 565°C |
Latrobe Lescalloy® 13-8 Mo VIM-VAR Precipitation Hardening Stainless Steel Lescalloy 13-8 Mo VIM-VAR is a precipitation hardening martensitic stainless steel offering excellent fracture toughness and transverse mechanical properties coupled with the resistance to stress-co.. |
|||
Tensile Strength, Ultimate | 1210 MPa | 175000 psi | Precipitation Hardened |
Special Metals NI-SPAN-C® Alloy 902 A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo.. |
|||
Tensile Strength, Ultimate | >= 1210 MPa | >= 175000 psi | |
Special Metals Nitinol High-Temperature Shape Memory Ni-Ti alloy Ribbon Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Tensile Strength, Ultimate | 1210 MPa | 175000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 20% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Tensile Strength, Ultimate | 1210 MPa | 175000 psi | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 40% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Tensile Strength, Ultimate | 1210 MPa | 175000 psi | |
Cytec Thornel® P-120 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |