Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1145 MPa | 166100 psi | |
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Ultimate | 1145 MPa | 166100 psi | |
Haynes 25 alloy, cold worked sheet, 15 % cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Ultimate | 1145 MPa @Temperature -73.0 °C |
166100 psi @Temperature -99.4 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Ultimate | 1145 MPa | 166100 psi | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |