Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Multibase Multi-Flex® TPE A 8002 BLK Multi-Flex® TPE 8002 is based on Shell's Kraton G polymer technology and is widely used in the automotive industry for applications requiring elastomeric performance with excellent ozone resistance.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.23.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used as an impact modifier or compatibilizer in polymer compounds. It ca.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Chevron Phillips KN 230 LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Chevron Phillips Marlex® 1409 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman PE1020 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium impact strength and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 .. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman PE1041 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good optical, medium impact strength, and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 2.. |
|||
Tensile Strength, Ultimate | 11.0 - 28.0 MPa | 1600 - 4060 psi | Average value: 20.3 MPa Grade Count:38 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Tensile Strength, Ultimate | 11.0 MPa @Thickness 2.00 mm |
1600 psi @Thickness 0.0787 in |
ASTM D4894 |
3M Dyneon™ TF 4246 PTFE 35% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Multibase Multi-Flex® D 3604 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Sylvin Technologies 8600-65 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Sylvin Technologies 9600-65 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 11.0 MPa @Temperature 70.0 °C |
1600 psi @Temperature 158 °F |
ASTM D638 |
Borealis Borstar® HE6081 Black Track Resistant HD Polyethylene Based Compound for Jacketing of Fiber Optical Cable Borstar HE6081 is based on high-density polyethylene and has a specially designed additive package to give excellent track resistance. It is also well protected against UV degradation in order to e.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Ecomass® 4702ZB92 Filled Polyurethane Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU) Base ResinFlexibleInformation provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Cytec EN-2541 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Dow HDPE 25455N High Density Polyethylene DOW HDPE 25455N resin is a narrow molecular weight distribution copolymer designed to offer good stress crack resistance and gloss with excellent toughness. This resin has good processability over a.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Dow HDPE 30460M High Density Polyethylene DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent pro.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Dow LDPE 722M Low Density Polyethylene DOW LDPE 722M resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent flexibility. Typical applications include c.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D412 |
Colorite Polymers Weatherflex™ CS1534WX (NTL01P) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Dow AMPLIFY™ GR 208 Maleic anhydride grafted (MAH) polymer AMPLIFY™ GR 208 Functional Polymer is a post reactor maliec anhydride grafted (MAH) polymer. The base polymer is an ethylene-butene copolymer exhibiting high flexibility and elasticity. It can be.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Colorite Polymers 92-623A General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Colorite Polymers Self Frosting™ 6011SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 4680 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Colorite Polymers 6012 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman Rexell® H2103 Injection Molding LLDPE
(discontinued **) Linear-low medium density homopolymer, injection molding, FDA compliant.Features: Good ESCR, low taste and order.Applications: Containers, closures, and ideal for blends and non-carbonated beverage .. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Colorite Polymers 6574 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | TM R050-36 |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | 500 mm/min (20 in./min.); Type IV Specimen; ASTM D638 |
Eastman D4042-P Polyethylene
(discontinued **) D4042-P is a low density resin designed for applications such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combination of high melt index and low.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman PE8020 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | TM R050-36 |
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Tensile Strength, Ultimate | 11.0 - 32.1 MPa | 1600 - 4650 psi | Average value: 20.8 MPa Grade Count:19 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |