Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 104 MPa | 15100 psi | 5 mm/min |
Arkema Group Rilsan® AZM 23 G9 T6LD Nylon 12, 23% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-050,(G+C)(F+D)(23+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Tensile Strength, Ultimate | 104 MPa | 15100 psi | ASTM D638 |
Chem Polymer Chemlon 113 G Nylon 66, 13% Glass Fiber Reinforced A 13% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials.Data provided by the manufacturer, .. |
|||
Tensile Strength, Ultimate | 104 MPa | 15100 psi | ASTM D638 |
A. Schulman ComAlloy E-13370B Internally Lubricated, Glass Fiber Reinforced Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |