Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1005 MPa
145800 psi
Haynes 188 alloy, plate at RT after 0 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Ultimate 1005 MPa
145800 psi
Haynes 188 alloy, plate at RT after 16000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Ultimate 1005 MPa
145800 psi
Haynes 214® alloy, 10% cold reduction, 925°C for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Ultimate 1005 MPa
145800 psi
Haynes 214® alloy, 20% cold reduction, 1095°C (2000°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Ultimate 1005 MPa
145800 psi
Haynes 230® alloy, 40% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Tensile Strength, Ultimate 1005 MPa
145800 psi
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 1005 MPa
145800 psi
Haynes 625 alloy, plate after 4000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..