Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1004 MPa | 145600 psi | |
Haynes Hastelloy® S alloy, gas tungsten arc welded, aged at 538°C (1000°F) for 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |