Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 957.0 MPa | 138800 psi | |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 1950°F (1070°C) Tensile strength (ultimate and yield), elongation, and hardness values are for samples annealed 1950°F (1070°C)/5 minutes/AC. This produces ASTM grain size 9.5. Other property values are ty.. |