Tensile Strength, Ultimate 9.20 MPa
1330 psi
ASTM D412
Multibase Multi-Flex® TPE A 9305 BLK
This product was developed for one shot airbag covers with improved stiffness and low temperature resistance. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 9.20 MPa
1330 psi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 451-87 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic flame retardant wire and cable elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethy..
Tensile Strength, Ultimate 9.20 - 33.0 MPa
1330 - 4790 psi
Average value: 18.9 MPa Grade Count:13
Overview of materials for Medium Density Polyethylene (MDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim..
Copyright © lookpolymers.com All Rights Reserved