Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 85.5 MPa | 12400 psi | ASTM D638 |
Technetics Group Amicon™ PET-P
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Tensile Strength, Ultimate | 85.3 MPa | 12400 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN333HRN Heat Resistant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Tensile Strength, Ultimate | 85.3 MPa | 12400 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN132VO Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |