Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 79.3 MPa | 11500 psi | ASTM D638-95 |
Multibase Multi-Pro® 4003 RC 40% Glass Filled Polypropylene Multi-Pro 4003 RC is a chemically coupled glass reinforced polypropylene compound suitable for engineered plastics applications due to its high heat, flexural and impact properties.Data provided by .. |
|||
Tensile Strength, Ultimate | 79.3 MPa | 11500 psi | ASTM D638 |
Nylene® 204 (HS) , Fast Cycle Nylon 6 Description: Nylene® 204 (HS) is a fast cycle, medium viscosity, nucleated nylon 6. 204 is UL approved and automotive approved. Information provided by Custom Resins.ALM, Nylene Canada, and Custom .. |
|||
Tensile Strength, Ultimate | 79.3 MPa | 11500 psi | ASTM D638 |
Nylene® 7139 (HS) Low Wear Nylon 6/6 Description: Nylene® 7139 (HS) is a general purpose, low wear, 1% MoS2 reinforced nylon 6/6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies o.. |
|||
Tensile Strength, Ultimate | 79.3 MPa | 11500 psi | ASTM D638 |
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6 Total Extractables < 1.5.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ASTM D651 |
Resinoid 1382 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ASTM D638 |
PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ASTM D638 |
PolyOne Edgetek® AS-10CF/000 ABS - 10% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 79.2 MPa | 11500 psi | ASTM D638 |
Firestone C212-15C Nylon 6, Heat Stabilized Off white color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ASTM D638 |
Firestone CR212-203-D Nylon 6, Heat Stabilized Black color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3 mm.Information provided by Firestone |
|||
Tensile Strength, Ultimate | 79.3 MPa | 11500 psi | ASTM D3574E |
Mearthane Durethaneâ„¢ F DF-640A Closed Cell Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |
|||
Tensile Strength, Ultimate | 79.3 MPa | 11500 psi | ASTM D3574E |
Mearthane Durethaneâ„¢ M DM-650A Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 95Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
Tensile Strength, Ultimate | 79.3 MPa | 11500 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4702-15 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Tensile Strength, Ultimate | 79.3 MPa | 11500 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4702-8 Polycarbonate EMERGEâ„¢ PC 4702-8 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat resi.. |
|||
Tensile Strength, Ultimate | 79.4 MPa | 11500 psi | ASTM D1708 |
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi.. |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | |
Covestro Bayblend® KU 2-1466 Polycarbonate/ABS Blend Flame retardant grade with 20% glass fiber reinforcement, high stiffness.Applications: Electrical industry.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated f.. |
|||
Tensile Strength, Ultimate | 79.3 MPa | 11500 psi | ASTM D638 |
Adell DR-12 10% Glass Reinforced Polycarbonate |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ATSM D638 |
Ashley Polymers Ashlene® 829 Nylon 6 Basic Nylon 6, low viscosity, unlubricated.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ATSM D638 |
Ashley Polymers Ashlene® ABS Resin R2018, 18% Glass Reinforced General purpose, 18% glass reinforced ABS resin.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ASTM D638 |
Chem Polymer Chemlon 212 Nylon 6, Lubricated, GP A medium viscosity, general purpose injection molding grade nylon 6. Internally lubricated for excellent mold release properties.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 105 Polypropylene, Glass Reinforced, Chemically Coupled, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ATSM D638 |
Ashley Polymers Ashlene® 828L Nylon 6 Medium viscosity general purpose nylon, complies with NSF under Standard 14 for pipe components.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ATSM D638 |
Ashley Polymers Ashlene® 829L Nylon 6 Basic Nylon 6, low viscosity, lubricated.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ATSM D638 |
Ashley Polymers Ashlene® 829LF Nylon 6 Basic Nylon 6, low viscosity, lubricated. This is FDA approved.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 284 PPO Alloy, Glass/Graphite Reinforced Data provided by the manufacturer, ComAlloy International Company.50% Glass/Graphite Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 79.0 MPa | 11500 psi | ASTM D638 |
PolyOne Lubri-Tech™ MP-20GF/15T Modified PPO - 20% Glass Fiber - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 79.0 MPa @Temperature 1149 °C |
11500 psi @Temperature 2100 °F |
|
Haynes 230® alloy, cold rolled and 1232°C solution annealed sheet Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |