Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20 wt.% glass ABS is highly resistant to weak acids and alkalis, and provides good resistance to most organic solvents. It is attacked by sulfuric and nitric acids, and is soluble in esters, ketones and ethylene .. |
|||
Tensile Strength, Ultimate | 75.8 MPa | 11000 psi | ASTM D882 |
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d.. |
|||
Tensile Strength, Ultimate | 75.8 MPa | 11000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PK-15GP/5T Polyetheretherketone (PEEK), PTFE Lubricated
(discontinued **) Description/Features:Graphite LubricatedPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, Dry As Molded
(discontinued **) AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resist.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
ExxonMobil Escor® AT-320 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components, such as aluminum foil, polyolefins, polycarbonate, PET, .. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
IDI Composites E-204 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Tensile Strength, Ultimate | 76.0 MPa @Temperature 22.0 °C |
11000 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | |
Haysite Ultratrac® H950 Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) This new generation of high performance material meets or exceeds all requirements for NEMA GPO-2 or GPO-3. ULTRATRAC ® H950 is recognized by U.L. as a 94V-0 material and offers greater arc and t.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Tensile Strength, Ultimate | 75.8 MPa | 11000 psi | |
Universal Wire Works 117 Nickel Alloy Welding Wire Alloy 117 is a nickel alloy electrode for welding nickel-chromium-cobalt-molybdenum alloys (UNS # N06617). This alloy electrode provides optimum strength and oxidation resistance above 1500 degrees .. |
|||
Tensile Strength, Ultimate | 75.84 MPa | 11000 psi | |
Abatron AboCast/AboCure 8109-6 High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat.. |
|||
Tensile Strength, Ultimate | 75.8 MPa | 11000 psi | ASTM D638 |
Adell BS-30 Nylon 6, General Purpose Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 76.0 MPa @Temperature 871 °C |
11000 psi @Temperature 1600 °F |
ASTM E8 |
ATI Allegheny Ludlum 310 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 213 Polystyrene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 75.8 MPa | 11000 psi | ATSM D638 |
Ashley Polymers Ashlene® 520 Nylon 66 A general purpose basic Nylon 66 resin, slightly lubricated.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 524 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Tensile Strength, Ultimate | 76.0 MPa | 11000 psi | Static |
Channel Industries 5400 Lead Zirconate Titanate Piezoelectric Navy Type ICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extens.. |
|||
Tensile Strength, Ultimate | 75.8 MPa | 11000 psi | |
Parylene Coating Services D Poly (P-Xylylene) Monomer is dichloro para-xylylene. Parylene D is recommended where high temperature resistance is needed; it can be used up to 140°C where oxygen is present.Parylene is a generic name for poly-par.. |
|||
Tensile Strength, Ultimate | 75.8 MPa | 11000 psi | ASTM D638 |
Adell RR-16 Copolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 75.8 - 121 MPa | 11000 - 17500 psi | Average value: 97.4 MPa Grade Count:4 |
Overview of materials for Acrylic, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o.. |