Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 75.08 MPa | 10890 psi | |
BCC Products MB 4000 RED Urethane Foundry Plank MB4000 Red is an extremely tough, high impact Urethane Plank, that can replace aluminum and other metals for many foundry applications. Features: excellent machinability, low dust emission, mostly .. |