Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.460 MPa
1082 psi
Dow Corning SILASTIC® 25786-V SILICONE RUBBER RED
60 Durometer, peroxide cured, high temperature resistance Silicone Rubber CompoundInformation provided by Dow Corning
Tensile Strength, Ultimate 7.460 MPa
1082 psi
Dow Corning SILASTIC® 37088-V SILICONE RUBBER RED
80 Durometer, peroxide cured, low compression set Silicone Rubber CompoundInformation provided by Dow Corning